andrewm wrote:
> John Griessen wrote:
>> I'm liking the transparency and low hassle and low toxicity of HCl/H2O2,
> I have been using CuCl for a bit over a year now and all I ever need to
> do is measure the acid levels and
> density and then top up with HCl or water to keep it in spec.
>
> Will still stain like FeCl, but you never need to neutralise it or throw
> anything away.
Thanks for that recipe and experience. The volume doesn't grow? Air
regenerates completely?
What's the rate like? I'm through 1 oz copper in <7 minutes at 105 deg
F with HCl/H2O2 etchant. Good for groups of proto boards.